<?xml version='1.0' encoding='UTF-8'?>
<?xml-model href="https://pds.nasa.gov/pds4/pds/v1/PDS4_PDS_1P00.sch" schematypens="http://purl.oclc.org/dsdl/schematron"?>
<?xml-model href="https://pds.nasa.gov/pds4/ctli/v2/PDS4_CTLI_1P00_2300.sch" schematypens="http://purl.oclc.org/dsdl/schematron"?>
<Product_Context xmlns="http://pds.nasa.gov/pds4/pds/v1" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xmlns:ctli="http://pds.nasa.gov/pds4/ctli/v2" xsi:schemaLocation="http://pds.nasa.gov/pds4/pds/v1 https://pds.nasa.gov/pds4/pds/v1/PDS4_PDS_1P00.xsd http://pds.nasa.gov/pds4/ctli/v2 https://pds.nasa.gov/pds4/ctli/v2/PDS4_CTLI_1P00_2300.xsd">
  <Identification_Area>
    <logical_identifier>urn:nasa:pds:context:instrument:em3.nanoindenter</logical_identifier>
    <version_id>1.3</version_id>
    <title>UNHT Nanoindenter</title>
    <information_model_version>1.25.0.0</information_model_version>
    <product_class>Product_Context</product_class>
    <Modification_History>
      <Modification_Detail>
        <modification_date>2026-07-07</modification_date>
        <version_id>1.3</version_id>
        <description>Removed duplicate Internal_Reference entries from Reference_List.</description>
      </Modification_Detail>
      <Modification_Detail>
        <modification_date>2025-12-24</modification_date>
        <version_id>1.2</version_id>
        <description>Adding missing "facility" references.</description>
      </Modification_Detail>
      <Modification_Detail>
        <modification_date>2025-12-24</modification_date>
        <version_id>1.1</version_id>
        <description>Updated schema version. Adding missing "facility" references.</description>
      </Modification_Detail>
      <Modification_Detail>
        <modification_date>2025-10-23</modification_date>
        <version_id>1.0</version_id>
        <description>Initial export from OLAF</description>
      </Modification_Detail>
    </Modification_History>
  </Identification_Area>
  <Reference_List>
    <Internal_Reference>
      <lid_reference>urn:nasa:pds:context:facility:laboratory.em3</lid_reference>
      <reference_type>instrument_to_facility</reference_type>
    </Internal_Reference>
  </Reference_List>
  <Instrument>
    <name>UNHT Nanoindenter</name>
    <Type_List_Area>
      <ctli:Type_List>
        <ctli:type>Mechanical Properties Instrument</ctli:type>
      </ctli:Type_List>
    </Type_List_Area>
    <description>The nanoindenter is a highly sophisticated instrument designed to measure the mechanical
properties of materials at the nanometer scale. It is a crucial tool in materials science, enabling 
researchers to explore the hardness, elastic modulus, and other mechanical properties of a wide array of 
materials with unprecedented precision through the nanoindentation process. 

The nanoindentation process involves loading a precisely shaped indenter, often made of diamond, into the 
material surface with a controlled force. This force is then held constant for a specified period to allow 
for any time-dependent deformation, followed by unloading the indenter while recording the material's 
response. During this process, the nanoindenter continuously records the load and displacement, generating 
a load-displacement curve that provides insights into the material's mechanical behavior. Key measurements 
include indentation hardness (H), which measures the material's resistance to plastic deformation and is 
expressed in gigapascals (GPa); it is calculated by dividing the maximum applied load by the projected 
contact area at that load and Indentation Modulus (M), which measures the material's stiffness and is also 
expressed in GPa; it is derived from the initial unloading slope of the load-displacement curve, considering 
the deformations of both the sample and the indenter.</description>
  </Instrument>